In case of the problem power consumption is on the high side, physical and standardcoal consumption is on the high side, the kiln temperature of clinker is higher, the consumption of ammonia is more than the normal in the #2 5000 t/d cement clinker production line,taking measures on the grate cooler, preheater system, kiln head,feeding scale of raw material and so on,dealing with system heat preservation and air leakage, adjusting ingredients, the effect of reconstruction is good. |